Degradation at the cathode-solid electrolyte interface limits high-energy-density sulfide-based allsolid-state batteries. For Ni-rich LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NCM622), cathode surface reduction and electrolyte oxidation are coupled through interfacial (electro-)chemical reactions. Although LiNbO 3 coatings are known to mitigate interfacial resistance growth, their effect on this coupling during operation remains unclear. Here, we combine operando X-ray absorption spectroscopy (XAS) and in situ X-ray photoemission electron microscopy (XPEEM) to follow the chemical evolution of the NCM622 surface and interfaces with Li 6 PS 5 Cl (LPSCl) with depth sensitivity and nanoscale spatial resolution. Already at open-circuit potential, reduced transition-metals, oxygendeficient domains and sulfate species co-localize where NCM622 particles contact LPSCl. Upon high-voltage charging, electrochemically inactive Ni 2+ , Co 2+ , and Mn 2+/3+ species become enriched at these contact regions, while oxygen depletion propagates inward across the particle surface. The LiNbO 3 coating suppresses transition-metal reduction, improves surface electrochemical activity by increasing surface Ni and Co oxidation and confines oxygen depletion to the contact regions. Residual degradation nevertheless persists, consistent with inhomogeneous LiNbO 3 coating coverage and its partial decomposition at high voltage. These findings provide nanoscale insight evidence that cathode and electrolyte degradation are interdependent and coupled through oxygen activity at the cathode surface and that effective coatings must suppress the cathode surface degradation.
No takes yet. Share an insight, caveat, or question.
Siller et al. (2026) studied this question.
Synapse has enriched 8 closely related papers on similar clinical questions. Consider them for comparative context: