Practical lithium‐sulfur (Li‐S) batteries require control of dissolved polysulfides, sulfur‐conversion kinetics, and lithium‐metal anodes under high sulfur loading and limited electrolyte. Dissolved molecular additives can influence all three processes, but their effects depend on concentration. Here, cyanuric chloride (CC) is examined from 0 to 0.10 M as an aprotic chlorotriazine additive with three ring‐nitrogen sites and three carbon‐chlorine centers. Spectroscopy suggests that 0.05 M (Optm‐CC) enhances nitrate (NO 3 − ) and bis(trifluoromethanesulfonyl)imide (TFSI − ) anions’ participation in Li‐ion solvation. This concentration reduces polysulfide crossover, enriches the sulfur‐cathode interphase with inorganic and triazine‐associated products, and promotes an inorganic‐rich, Cl‐containing interphase at the lithium‐metal anode. As a result, these changes lower cyclic‐voltammetry peak separation to 0.191 V, raise the apparent Li|Li exchange‐current density to 0.203 mA cm −2 , support Li|Li symmetric‐cell cycling for over 1100 cycles, deliver 560 mAh g Sulfur −1 at 10C, and sustain 3000 Li‐S cycles. Increasing the CC concentration to 0.10 M (Conc‐CC) produces a larger spectroscopic shift, but the apparent Li‐ion transference number and lithium‐electrode polarization deteriorate. Furthermore, a pouch cell operated at 8 mg Sulfur cm −2 and 5 µL mg Sulfur − 1 retains 72.73% of its stabilized capacity after 300 cycles. Among the tested formulations, 0.05 M best balances coordination, interphase chemistry, and electrochemical performance.
No takes yet. Share an insight, caveat, or question.
Ardhi et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: