Thermally stable load transfer remains a central challenge for aluminum matrix composites because matrix softening and interfacial degradation impair high-temperature performance. Here, an Al3BC-mediated SiC/Al composite exhibits superior stiffness and strength through elastic-plastic partitioning. At 350°C, it retains a modulus of 92.1 GPa and ultimate tensile strength of 190 MPa, corresponding to a specific modulus of 32.7 GPa·cm3/g and specific strength of 67.4 MPa·cm3/g. Post-deformation characterization reveals a structurally stable, dislocation-poor SiC@Al3BC framework, while Al2O3-rich regions store deformation-induced dislocations. These complementary roles establish a transferable strategy for lightweight, heat-resistant aluminum matrix composites with distinct elastic load-bearing and plastic accommodation functions.
No takes yet. Share an insight, caveat, or question.
Hu et al. (2026) studied this question.
Synapse has enriched 8 closely related papers on similar clinical questions. Consider them for comparative context: