Answers are grounded in this paper and cite their sources.
Castable nanostructured alloys (CNAs) offer a scalable route to extend the high-temperature capability of reduced-activation ferritic/martensitic steels, yet their strain-accommodation behavior at 650 °C remains unclear. Under the present test condition, the CNA-derived RAFM steel exhibited a yield stress of 481.2 MPa, an ultimate tensile strength of 567.3 MPa and a total elongation of 26.18%. In-situ DIC, EBSD and TEM reveal a coupled response: MX/M23C6 interfaces and lath/sub-grain boundaries store dislocations, recovery-assisted rearrangement preserves matrix accommodation, and subsequent deformation is progressively confined to a necking zone. This interface-mediated hierarchy delays localization and produces the favorable 650 °C strength–ductility balance.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: