The transition toward low-carbon construction materials has intensified interest in alkali-activated materials (AAMs), yet the systematic selection of suitable precursors from locally available by-product streams remains a critical and underexplored challenge. This paper presents a two-stage screening methodology for evaluating industrial and urban by-products as AAM precursors, combining a macro-scale opportunity analysis with a laboratory-scale suitability assessment, and applies it to a case study territory in Spain. The opportunity analysis screens nine candidate materials against criteria of generation volume, geographic distribution, conditioning requirements, compositional variability and occupational hazard profile. The suitability analysis applies a consistent set of characterisation techniques, comprising X-ray fluorescence (XRF), X-ray diffraction with Rietveld refinement (XRD-R), ²⁹Si and ²⁷Al solid-state nuclear magnetic resonance (SS NMR) and BET specific surface area, followed by a selective alkaline dissolution test with ICP-OES determination of released Si and Al and a preliminary activation and mechanical assessment on pastes. Based on these analyses, four compositional groups are identified: high-silicon materials (waste glass and glass sludge), low-silicon/high-calcium materials (ladle furnace slag, LFS), aluminium-rich/calcium-free materials (spent fluid catalytic cracking catalyst) and hybrid aluminosilicates (ceramic construction and demolition waste). The results show that amorphous content is not correlated with silicon content, and that neither bulk composition, nor amorphous content, nor the silicate polymerisation state revealed by SS NMR predicts the silicon and aluminium actually released in alkaline medium or the strength developed on activation under the conditions tested. LFS, the most depolymerised material of the set, releases the least silicon in absolute terms, because its silicon content is low and close to half of it is bound in crystalline dicalcium silicate. LFS and spent FCC catalyst failed to consolidate under the common activation protocol applied here, which does not show that they cannot be activated under conditions suited to each of them. On the combined evidence, and as a preliminary ranking that depends on the activation conditions used, non-recyclable container glass cullet, fired ceramic tile waste and ceramic CDW red clay brick are identified as the most viable precursors. The study assesses precursor suitability and early-age behaviour; it does not address dissolution kinetics, precursor-specific optimisation of activation conditions, the variability of each source over time, long-term durability or full mix performance. The proposed two-stage procedure is transferable to other territorial or industrial contexts, although the specific rankings reported here depend on the regional dataset and on the activation conditions used.
No takes yet. Share an insight, caveat, or question.
Garcia-Díaz et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: