Answers are grounded in this paper and cite their sources.
Recycled aggregate concrete (RAC) offers significant environmental benefits but is often limited by high porosity, weak interfacial transition zones, and reduced mechanical and durability performance. This study evaluated the long-term effects of metakaolin (15%), an aluminosilicate mineral derived from kaolin clay, silica fume (7.5%), a metallurgical by-product of silicon and ferrosilicon smelting and polypropylene fibers (PPFs, 0–1.5%) on RAC containing 0%, 50%, 75%, and 100% recycled coarse aggregate (RA), a mineral residue stream from construction and demolition waste. Sixteen concrete mixtures were produced, and 768 cylindrical specimens were tested for slump, compressive strength, split tensile strength, water absorption, sulfuric acid resistance, ultrasonic pulse velocity, rebound number, and microstructural characteristics up to 180 days. Increasing RA and PPF contents reduced workability, with slump decreasing from 98 mm to 40 mm. The mixture containing 1% PPF and 0% RA achieved the highest 180-day compressive and split tensile strengths of 64.4 MPa and 6.9 MPa, respectively, while the corresponding 50% RA mixture attained 46.6 MPa and 5.1 MPa. Under sulfuric acid exposure, 1.5% PPF reduced the 180-day mass loss of the 50% RA mixture from 23% to 14%. SEM and nondestructive tests confirmed improved matrix densification, interfacial bonding, and crack bridging. Overall, 1% PPF with 50% RA provided the best balance between strength, durability, and sustainability for structural concrete applications. The enhanced sulfuric acid resistance is particularly beneficial for mining and mineral processing infrastructure exposed to aggressive acidic environments, such as acid mine drainage, sulfide-rich tailings, and metallurgical plant floors
No takes yet. Share an insight, caveat, or question.
Al-Naghi et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: