Low-temperature tempering (LTT) is a widely used heat treatment for reheated and quenched (RQ) ultrahigh-strength steels to improve their mechanical properties and reduce susceptibility to hydrogen embrittlement (HE). While LTT is typically applied to RQ steels, this study investigates its effect on the HE resistance of a lath-martensitic, direct-quenched (DQ) steel. LTT with different holding times at 200°C was applied, and HE susceptibility was evaluated using in-situ constant-displacement tuning-fork tests (TFT) until fracture, complemented by standard hydrogen permeation tests to measure hydrogen diffusivity. Results show that LTT accelerates hydrogen diffusion and shifts the cracking mechanism from quasi-cleavage to partially ductile microvoid coalescence, prolonging both crack initiation and time to fracture. The observed improvement in HE resistance may be associated with carbon redistribution, which is proposed to reduce dislocation mobility and alter hydrogen trapping at dislocations.
No takes yet. Share an insight, caveat, or question.
Latypova et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: