Answers are grounded in this paper and cite their sources.
The use of steel slag aggregates in concrete supports waste valorisation and sustainable construction, but their poor volumetric stability causes expansion-induced cracking and concrete deterioration. A novel carbonated cement coating was developed through three cycles of cement packaging and carbonation curing. Carbonated cement-coated slag (CCS) was evaluated against water-cured hydrated cement-coated slag (HCS). Mercury intrusion porosimetry and X-ray diffraction characterised the coating’s pore structure and phases; aggregate properties, concrete strength and long-term stability were evaluated. Carbonation reduced coating porosity from 20% to 16% and converted portlandite to calcite and vaterite, forming a denser, more robust coating. Relative to HCS, CCS reduced water absorption from 3.63% to 2.75%, crushing value from 5.14% to 4.07% and autoclave pulverisation rate from 1.82% to 1.07%. CCS concrete reached 41.3 MPa and 51.5 MPa at 7 days and 28 days, respectively. During elevated-temperature curing, it maintained an intact surface and gained strength to 58.8 MPa at 90 days, whereas concrete containing untreated steel slag lost strength and deteriorated. These results demonstrate that carbonation rapidly creates a dense, robust coating that suppresses steel slag expansion, improves aggregate and concrete performance and supports large-scale steel slag utilisation in durable, sustainable concrete.
No takes yet. Share an insight, caveat, or question.
Liu et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: