This study examines the combined effect of waste glass powder (WGP) and alkali-treated sisal fiber (SF) on the fresh and hardened properties of M20 concrete and develops a multi-output artificial neural network (ANN) that predicts compressive, splitting tensile and flexural strength simultaneously. Twenty-five mixes (WGP 0–20%, SF 0–2% of the binder mass; w/b = 0.50) were tested, with ten specimens per mix and test (750 specimens). SF1.5_WGP15, the best-performing formulation tested, reached 33.0, 4.8 and 6.1 MPa, about 17%, 35% and 39% above the control. Two-way ANOVA showed significant WGP and SF effects on all three strengths and a significant interaction for compressive and splitting tensile strength. A hybrid dataset of 2,500 records was assembled from the experiments, peer-reviewed studies and synthetic records interpolated from the measured response surfaces. On the test subset, the ANN gave R² = 0.941, 0.937 and 0.921 (RMSE = 0.85, 0.12 and 0.14 MPa), comparable to Random Forest and slightly below Gradient Boosting. In grouped cross-validation, with whole mixes withheld and synthetic records regenerated from the training mixes only, the ANN reached R² = 0.54–0.64 for unseen mixes. The model applies only to M20 concrete with w/b = 0.50 at 28 days, within 0–20% WGP and 0–2% SF.
No takes yet. Share an insight, caveat, or question.
Anandaraj et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: