Answers are grounded in this paper and cite their sources.
To investigate the effect of annealing temperature on interface evolution, microstructure and the mechanical properties of Al/Mg/Al laminated composites (LMCs), LMCs fabricated by flat rolling at 400 °C were annealed at 200, 250, 300, 325, 350 and 375 °C for 60 min. Scanning electron microscopy (SEM), energy-dispersive spectroscopy (EDS), X-ray diffraction (XRD), electron back-scatter diffraction (EBSD), transmission electron microscopy (TEM), as well as tensile, cupping, peeling and hardness tests were employed to characterize their interfacial structure, microstructure and mechanical properties. With increasing annealing temperature, the interface gradually transforms from mechanical interlocking to metallurgical bonding, and the intermetallic compound (IMC) layer thickens continuously. Excessive elemental interdiffusion causes interfacial embrittlement at 375 °C. The Mg layer undergoes recovery, recrystallization, and grain growth, accompanied by changes in crystallographic texture. In contrast, the Al layer possesses a higher recrystallization temperature; it maintains a deformed microstructure at low temperatures and exhibits prominent recrystallization only at 350 °C. The dislocation density of both layers decreases first and then increases, reaching the minimum value at 350 °C. In terms of mechanical properties, the yield strength (YS) decreases monotonically with rising annealing temperature, and the yield-to-tensile ratio (ratio of yield strength to ultimate tensile strength, σs/σb) declines correspondingly. The work-hardening exponent reaches a peak value of 0.291 at 350 °C. Elongation (EL) increases first and then fluctuates at a high level (10.2% at 350 °C). The peeling strength varies in a non-monotonic trend: it presents the maximum value of 12.3 N/mm at 200 °C, drops to the minimum of 1.1 N/mm at 325 °C, and rebounds to 4.1 N/mm at 350 °C and 8.1 N/mm at 375 °C. For stamping formability, the Erichsen cupping index (IE) is the lowest (2.12 mm) at 200 °C and stabilizes within the range of 3.15–3.31 mm above 250 °C. In summary, favorable comprehensive performance is obtained under the annealing condition of 350 °C/60 min, with σs/σb of 0.733, an IE of 3.27 mm and a peeling strength of 4.1 N/mm. This condition exhibits good comprehensive formability and provides an experimental basis for the annealing-process design of LMCs.
No takes yet. Share an insight, caveat, or question.
Duan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: