Answers are grounded in this paper and cite their sources.
Porous methyl-modified silica anti-reflective coatings were prepared by an acid-catalysed sol‑gel route and evaluated for high-temperature solar applications. Four formulations (S5-S8) were obtained from tetramethoxysilane (TMOS) combined, respectively, with methyltrimethoxysilane (MTMS), methyltriethoxysilane (MTES), dimethoxydimethylsilane (DMDMS), or diethoxydimethylsilane (DEDMS). The sols were prepared at pH approximately 1.5, stirred for 50 min, aged for at least 30 h, deposited by drop-coating and/or dip-coating on 10CrMo9.10 heat-resistant steel, and thermally treated at 60, 400, and 500 °C. Reflectance was measured with a Lambda 950 UV/Vis/NIR spectrophotometer over 300-800 nm. The arithmetic mean reflectance decreased from 12.89 to 8.51% for S5, from 15.02 to 8.12% for S6, from 22.57 to 11.83% for S7, and from 14.42 to 9.58% for S8 between the 60 and 500 °C conditions. S7 and S8 reached their lowest mean reflectance at 400 °C (11.05 and 9.22%, respectively), indicating a non-monotonic response at the highest temperature. S5 formed the most compact coating, whereas S7 exhibited cracking and local exfoliation; measured coating thicknesses ranged from 45.9 to 231.7 µm. The study therefore characterises composition- and temperature-dependent coating behaviour rather than claiming formal optimisation of the anti-reflective process.
No takes yet. Share an insight, caveat, or question.
Ciurel et al. (2026) studied this question.
Synapse has enriched 8 closely related papers on similar clinical questions. Consider them for comparative context: