In sulfur‐vulcanized nitrile butadiene rubber (NBR), the crosslink type distribution governs mechanical performance, yet post‐curing is rarely used to control it. This study examines two‐stage vulcanization, a shortened in‐mold cure followed by post‐curing at 130°C, in a silica‐filled industrial NBR. Mold temperature (150°C and 170°C), cure time and post‐curing duration (1 and 4 h) were varied. Multi‐stage swelling analysis was combined with hardness, compression set, tensile, dynamic‐mechanical, and fatigue properties. In the most undercured samples, 1 h of post‐curing reduced the polysulfidic fraction from 43% to below 10% and raised the monosulfidic fraction from 27% to above 85%, whereas the apparent crosslink density changed only moderately. This restructuring raised hardness from 71 to 80 Shore A, reduced compression set and damping, but increased crack growth rates in initially undercured samples. Vacuum post‐curing reproduced the crosslink density increase and the reduced elongation at break observed in air; these changes therefore arise from sulfur maturation rather than thermo‐oxidative aging, with oxygen adding stiffening confined to the low‐strain modulus. Two‐stage curing thus enables targeted modification of the NBR crosslink type distribution, with energy and throughput benefits where the resulting properties meet application requirements.
No takes yet. Share an insight, caveat, or question.
Hufnagl et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: