Answers are grounded in this paper and cite their sources.
In this investigation, a thrust ball-on-flat electric discharge test rig was used to examine the progression of electrically induced bearing damage. Tests were conducted at Hertzian contact pressures of 2, 3, and 4 GPa under a constant lambda ratio of 6 and a fixed electrical power of 3 W per rolling element. Specimens were tested with and without electrical power at increasing cycle counts and examined using optical microscopy, optical surface profilometry, and near-surface yield-strength measurements. Surface discoloration observed after 5e6 cycles indicated evidence of localized heating and tempering of the material caused by electrical power. The electrothermal process reduced the near-surface yield strength by 16%. Two distinct damage modes were observed in the running track: (i) central track deformation and (ii) discharge-induced pitting. The results demonstrate that, at 4 GPa, the threshold for permanent surface deformation was reached at a cycle count approximately two orders of magnitude lower with electrical power than without. Pit initiation and growth were evaluated using a defined pitting criterion (50 μm width x 1 μm depth) and mapped using S–N diagrams. The results showed that electrothermally induced material softening promoted earlier pit initiation and subsequent pit growth. Accordingly, the presence of electrical power reduced the cycles to failure by up to 80% relative to tests conducted without electrical power.
No takes yet. Share an insight, caveat, or question.
Park et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: