Answers are grounded in this paper and cite their sources.
Sol-gel derived chitosan-modified BTESPT silane composite coatings were fabricated on aluminum alloy substrates. The effects of chitosan concentration on the surface morphology and corrosion resistance were investigated. The optimal coating contained 1.0 g/L chitosan, achieving a polarization resistance of 2.919 × 10 7 Ω·cm 2 and a corrosion current density of 3.07 × 10⁻ 10 A·cm⁻ 2 . The corresponding protection efficiency reached 99.98%. XPS analysis confirmed a Si content of 15.66 at%, exceeding that of the pure BTESPT coating (10.55 at%), with complete scratch filling observed. XPS further detected Si 4+ -O and Al-O bonds, suggesting chemical interactions at the coating-substrate interface. Insufficient chitosan (0.5 g/L) resulted in incomplete film coverage and its polarization resistance (3.979 × 10 5 Ω·cm 2 ) fell below that of the bare alloy. Excessive chitosan (≥1.5 g/L) introduced pore defects. Warburg impedance characteristics appeared in the low-frequency EIS region. The polarization resistance dropped to the 10 6 Ω·cm 2 range. This synergistic corrosion protection arises from the interplay among a dense silane barrier, interfacial Si 4+ -O/Al-O bonding, and cathodic inhibition.
No takes yet. Share an insight, caveat, or question.
Chen et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: