: The effect of heating rate prior to intercritical annealing on the microstructural evolution, retained austenite (RA) stability, and mechanical properties of a 0.16C–4.7Mn–1.6Al–0.2Si–0.2Mo medium-Mn steel was investigated. Complex dilatometric, X-ray diffraction, SEM, EBSD, TEM, and STEM-EDS analyses were performed on specimens heated at rates ranging from 0.1 to 100 °C/s and subsequently annealed at 680 °C for up to 5 h. Increasing the heating rate suppressed martensite tempering and carbide precipitation prior to entering the intercritical region, resulting in a more chemically homogeneous and highly defected martensitic matrix. In contrast, slow heating promoted the formation of Mn- and C-enriched M 23 C 6 and M 3 C carbides, generating pronounced chemical heterogeneity. Although prolonged annealing substantially reduced the differences in the ferritic matrix, pronounced differences remained in RA morphology and stability. Slow heating resulted in fine and isolated RA grains, whereas rapid heating promoted the formation of coarser and increasingly interconnected RA regions. Quantitative two-dimensional connectivity analysis supported this morphological transition: the fraction of the total retained-austenite area contained in the ten largest connected regions increased from 26.3 ± 1.3% at 0.1 °C/s to 70.4 ± 3.0% at 100 °C/s, while the number of connected retained-austenite regions decreased from 848 ± 39 to 418 ± 24. After 5 h of annealing, the RA fraction increased from 33.2 to 38.1 vol.% with increasing heating rate. Over the same heating-rate range, hardness increased from 264 to 275 HV1. In the tensile-test series, increasing the heating rate from 1 to 100 °C/s increased the ultimate tensile strength from 762 to 847 MPa. Dilatometric and microstructural analyses further revealed that RA formed after rapid heating exhibited lower thermal and chemical stability despite its higher volume fraction. The results demonstrate that the heating rate controls the competition between carbide precipitation and austenite reversion, leading to a persistent microstructural memory of the thermal path that remains active even after prolonged intercritical annealing. These findings identify heating rate as an effective parameter for tailoring retained austenite morphology, stability, and mechanical performance during continuous annealing of medium-Mn steels.
No takes yet. Share an insight, caveat, or question.
Skowronek et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: