Ni and Al alloyed hot‐work tool steel (HNA steel) was developed to improve the hardness–toughness balance and mitigate carbide coarsening during tempering. After quenching at 1040 °C and tempering at 540–590 °C, HNA steel exhibited a pronounced secondary‐hardening response. At the secondary‐hardening peak of 560 °C, the hardness reached approximately 58.44 HRC while the room‐temperature unnotched impact energy was approximately 214.95 J. HRTEM/FFT and STEM‐EDS observations support the presence of finely dispersed NiAl‐type B2 nanoprecipitates with an average size of approximately 5.9 nm. Their fine dispersion and good crystallographic compatibility with the bcc martensitic matrix are consistent with dislocation pinning, suppressed recovery, and martensitic stabilization. Over 540–590 °C, the average carbide size increased from 144.24 to 457.72 nm in HNA steel and from 200.24 to 566.63 nm in H13 steel. The LSW‐derived comparative coarsening parameter K of HNA steel was approximately 22%–53% of that of H13 steel under identical tempering conditions. The improved temper‐softening resistance and hardness–toughness balance are associated with the combined effects of alloying, NiAl‐type B2 nanoprecipitation, carbide refinement, and stabilization of the tempered martensitic matrix.
No takes yet. Share an insight, caveat, or question.
Xing et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: