Answers are grounded in this paper and cite their sources.
Au-Fe2O3 heterostructure nanoparticles were synthesized via liquid-phase laser ablation to study how different routes affect their morphology and plasmonic response, specifically comparing two reversed target-colloid configurations, a parameter scarcely explored in these hybrid systems. Eight samples were prepared using two colloid/target configurations: ablation of a metallic gold target in Fe2O3 nanoparticle colloid or ablation of a Fe2O3 target in a preformed Au nanoparticles colloid. Water and acetone medium were used, with laser fluences of 0.23 and 0.39 J cm−2, and ablation times of 4 and 10 min under 532 nm irradiation. TEM micrographs showed morphology dependence on colloid/target configuration. Au colloid-derived samples had quasi-spherical or ellipsoidal nanoparticles, while Fe2O3 colloid-derived samples showed heterogeneous structures including surface-decorated-like particles, core–shell-like structures, irregular aggregates, and rings. UV-vis analysis revealed differences: Au colloid samples retained a clear LSPR signal at 521–539 nm (FWHM 62–113 nm), but only one Fe2O3 colloid sample showed a broadened band at 568 nm, with other Fe samples lacking a distinct LSPR. These optical differences aligned with TEM findings. XPS analysis showed Au 4f spectra dominated by a single doublet consistent with predominantly metallic Au, without resolved higher-binding-energy components attributable to oxidized Au species. Multiplet-based fitting of the Fe 2p spectra revealed Fe(III) as the dominant oxidation state, with smaller Fe(II) contributions.
No takes yet. Share an insight, caveat, or question.
Ramírez et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: