Fracture precursor identification in semi-flexible pavement (SFP) materials requires quantitative interpretation of acoustic emission (AE) and mechanical responses. Semi-circular bending tests on unmodified (PK) and KH550-modified (KH) SFP materials were analyzed at −10 °C, 0 °C, and 25 °C. Three independently tested specimens were included for each material–temperature condition, yielding 18 specimens. The historic index (HI), Sentry function, and normalized energy difference η *(t) characterized damage-related acoustic activity. Precursors were identified retrospectively when the backward-window rate of η *(t) exceeded an adaptive baseline threshold at three consecutive points. From −10 °C to 25 °C, the mean maximum HI decreased by 71.2% for PK and 78.7% for KH, accompanied by more temporally distributed AE activity. Under the reference settings, precursors were identified in all 12 specimens at −10 °C and 0 °C and four of six at 25 °C. Across nine parameter combinations, detection counts were 108/108 and 44/54, respectively, representing repeated evaluations rather than independent tests. The mean lead times among detected specimens ranged from 2.80 to 4.60 s at the two lower temperatures and 5.94 to 8.54 s at 25 °C. The criterion showed reduced detection robustness at 25 °C and, owing to peak-state normalization, remains an offline assessment rather than a validated real-time warning system.
No takes yet. Share an insight, caveat, or question.
Song et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: