Answers are grounded in this paper and cite their sources.
A 6% concrete-latex addition raised the Marshall stability of submerged asphalt wearing course by 37% and its elastic modulus by 35% on average, and a simple life-cycle scenario shows how that can prevent road waste. Pavements in the flood-prone Niger Delta are repeatedly saturated, fail early, and are then milled and replaced, generating asphalt waste and consuming virgin aggregate and bitumen. This article takes the waste-management view of a laboratory study in which asphalt concrete was modified with 0–10% concrete latex and immersed for 0–7 days. The 6% mix retained higher stiffness at every immersion time (for example, 5,119 MPa after 7 days against 3,629 MPa unmodified), and, using the Asphalt Institute fatigue criterion, its estimated fatigue life was 1.20–1.31 times that of the unmodified mix. In a transparent scenario for a 7.3 m wide, 50 mm wearing course, a life-extension ratio in that range avoids about 200–800 t of milled asphalt waste per kilometre over 24 years, after counting the extra latex used, with a break-even at about 1.06. The latex is found at the top of the waste hierarchy (prevention) and is used in conjunction with the waste-based modifiers (polythene, polystyrene, ashes and recycled dust) discussed at Rivers State University. The results support SDG 9, 11, 12 (especially target 12.5) and 13.
No takes yet. Share an insight, caveat, or question.
Igwe et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: