Answers are grounded in this paper and cite their sources.
Additively manufactured Ti6Al4V lattice structures are promising for biomedical applications, but partially melted powder particles and surface defects from Direct Metal Laser Sintering may adversely affect their properties. This study evaluated a three-stage post-processing strategy comprising wet chemical etching (in aqueous acid solution), plasma etching and diamond-like carbon (DLC) coating deposition. Hydrofluoric acid (HF) concentration and etching time were evaluated for powder removal, mass loss and mechanical properties, followed by assessment of surface and biological properties. The most favorable HF treatment was 1.4% HF for 7 min, effectively removing powder particles but causing 14.53% mass loss and a 14.69% reduction in load-bearing capacity at 0.2% strain. Plasma etching resulted in less than 0.2% mass loss and, when applied after chemical etching, removed surface defects and reduced roughness without changes in lattice geometry. DLC coatings exhibited an amorphous carbon structure with an ID/IG ratio of 1.18 ± 0.01. The highest open-circuit potential was obtained for DLC-coated samples (56 ± 34 mV), exceeding that of unmodified samples (22 ± 63 mV). All variants were non-cytotoxic according to ISO10993-5, while the highest surface colonization by Saos-2 cells was observed after deposition of a DLC coating through a comparative analysis of their growth on the solid region of 3D-printed samples. Overall, the sequential treatment enabled the functional properties of Ti6Al4V lattice structures to be tailored beyond the scope of conventional surface cleaning.
No takes yet. Share an insight, caveat, or question.
Grabarczyk et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: