This study investigates the influence of calcination temperature and duration on the structural, optical, and photocatalytic properties of lanthanum ferrite (LaFeO 3), synthesized via the sol–gel method using lanthanum and iron nitrates and citric acid as a complexing agent. The precursor was calcined at 850°C for 5, 7, and 10 h and at 900°C for 5 and 7 h. The resulting samples were characterized by FTIR, XRD, and UV–visible. FTIR spectra revealed a characteristic Fe–O vibration band at approximately 560 cm − 1, while XRD confirmed the orthorhombic perovskite structure (space group Pnma) in all samples. The sample calcined at 900°C for 5 h exhibited the smallest crystallite size (40.32 nm) and the lowest optical band gap (2.32 eV). Under visible‐light irradiation, this sample achieved 31% methylene blue (MB) removal after 300 min, with an apparent zero‐order rate constant of 0.0115 mg L − 1 min − 1. Photocatalytic performance was strongly influenced by the initial solution pH, reaching approximately 97% MB removal at pH 8. This enhancement is attributed to electrostatic attraction between cationic MB molecules and the negatively charged LaFeO 3 surface above its point of zero charge. These findings highlight the potential of LaFeO 3 perovskite for visible‐light‐driven wastewater treatment.
No takes yet. Share an insight, caveat, or question.
Chakour et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: