Closed-cell AA7075 composite foams containing 0–3 wt.% Si3N4 were produced by liquid-state foaming with TiH2 heat-treated at 520 °C for 2 h, which shifted its main hydrogen release by ≈85 °C to ≈650 °C. The effect of Si3N4 on the cellular architecture and quasi-static compressive behaviour (ISO 13314) was investigated. Compared with the unreinforced foam (0.44 g cm−3, 84.5% porosity, median pore diameter 1.54 mm), the foams with 1–3 wt.% Si3N4 had densities of 0.52–0.73 g cm−3, porosities of 81.3–74.2% and median pore diameters of 0.52–1.00 mm. XRD and SEM–EDS confirmed that Si3N4 was retained after foaming. As the relative density increased from 0.155 to 0.258, the yield strength rose from ≈11 to ≈46 MPa, the plateau stress from ≈9 to ≈43 MPa, the compressive strength from ≈14 to ≈67 MPa and the energy absorbed up to 50% strain from 4.1 to 18.8 MJ m−3, while the densification strain increased from ≈0.55 to ≈0.88. The plateau stress followed a Gibson–Ashby power law with an exponent of 2.64 (R2 = 0.955; 16 specimens). Collapse changed from localised shear banding in the low-density foams to layer-by-layer crushing in the Si3N4-richer foams. The specific plateau stress of the 3 wt.% foam (≈59 MPa cm3 g−1) exceeded that of reported AA7075-based composite foams, showing that small Si3N4 additions allow the plateau stress of AA7075 foams to be tuned for lightweight energy absorbers.
No takes yet. Share an insight, caveat, or question.
Kanth et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: