As a critical optical component, achieving crack‐free surfaces on fused silica through CO 2 laser polishing remains challenging due to residual stresses induced by steep thermal gradients. This study aims to elucidate the mechanisms of crack initiation and propagation during this process. A three‐dimensional multiphysics model coupling temperature and stress fields was developed and validated experimentally (< 5% error). Crack propagation was simulated using the extended finite element method (XFEM), analyzing the effects of crack size, location, and interaction. The maximum residual von Mises stress after laser polishing was 26.35 MPa. Combined with the subsequent XFEM fracture analysis, the results suggest that crack development cannot be attributed to the overall residual stress level alone and that pre‐existing defects play an important role in crack initiation and propagation. Terminal‐edge cracks exhibited significantly greater propagation (e.g., 1380 μm for a 100‐μm crack) than central cracks due to heat accumulation. Collinear cracks showed a 51% reduction in propagation length (340 μm vs. 700 μm) due to stress shielding. Implementing a 900°C isothermal preheating strategy effectively reduced the thermal gradient, suppressing crack propagation length by 70% (from 400 to 120 μm).
No takes yet. Share an insight, caveat, or question.
Lu et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: