This study investigates the effects of welding Hardox 450 (martensitic steel) to Optim 700 MC (high-strength structural steel) and of subsequent post-weld heat treatment (PWHT) on hardness and corrosion behavior. The metal active gas (MAG) welding method was used for the welding process. After welding, the samples were subjected to heat treatment at 150, 300, and 450 °C. Following the heat treatment, potentiodynamic polarization measurements were performed on the samples in a 3.5 % NaCl solution. Subsequently, the microstructure and hardness of the heat-affected zone (HAZ) of the samples were evaluated. The results showed that welding caused localized hardness increases in the HAZ of Hardox 450 steel. PWHT significantly reduced these localized hardness increases in the HAZ and increased corrosion resistance. While the lowest corrosion rate was obtained in the sample subjected to PWHT at 300 °C, PWHT at 450 °C was determined to be the optimum condition for toughness and electrochemical corrosion behavior. This study emphasizes that PWHT should be carried out under appropriate conditions to improve the mechanical properties and corrosion resistance of weld zones in high-strength steels.
No takes yet. Share an insight, caveat, or question.
İpek et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: