Aluminum matrix composites combining Al–Fe intermetallic strengthening with the hardness of B 4 C are promising for lightweight structural applications, yet solid-state processing of the ternary Al–Fe–B 4 C system remains insufficiently explored. In this study, Al–10 wt.% Fe composites containing 0, 5, and 10 wt.% B 4 C were mechanically alloyed for 0, 2, and 15 h, cold-pressed at 600 MPa, and microwave-sintered at 600 °C for 1 h. Phase evolution, powder characteristics, microstructure, density, hardness, and compressive behavior were evaluated. No intermetallic reflections were detected in the mechanically alloyed powders; B 4 C promoted particle and coherent diffraction domain refinement, although 10 wt.% B 4 C combined with 15 h milling caused agglomeration. During sintering, Al 13 Fe 4 formed in situ, while minor Fe 3 C and B phases indicated partial mechanochemical decomposition of B 4 C. Relative density decreased with increasing B 4 C content and reached a minimum of 89.27 % for the 2 h milled Al–10Fe–10B 4 C composite. The 15 h milled Al–10Fe–10B 4 C composite exhibited the highest microhardness (2.381 GPa), whereas the highest compressive strength (199.8 MPa) was obtained after 2 h milling. Overall, mechanical alloying combined with microwave sintering enhanced local strengthening, while residual porosity and agglomeration limited bulk mechanical performance.
No takes yet. Share an insight, caveat, or question.
İndi et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: