Composite single-bolt double-shear joints with prefabricated hole-edge delamination are systematically investigated through experimental and numerical approaches. Tensile tests are conducted on specimens with delamination diameters of 0, 12, 20 and 28 mm. A three-dimensional progressive damage model incorporating the Hashin-type failure criterion and Camanho degradation model is developed using a UMAT subroutine, with cohesive elements introduced to simulate delamination. Numerical predictions agree well with experiments, with errors within 10%. Parametric studies reveal that delamination location, shape, and orientation all significantly affect joint performance. Small delaminations propagate extensively beyond their initial region, whereas large delaminations exhibit limited propagation beyond the prefabricated defect. The ultimate load decreases by 5.7% as the delamination diameter increases from 0 to 28 mm. The proposed method provides a reliable tool for damage-tolerant design of composite bolted joints.
No takes yet. Share an insight, caveat, or question.
Li et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: