Diesel engine pistons experience non-uniform and cyclic thermal loading, and excessive crown heating raises the temperature of the aluminium substrate. Coating selection based only on steady temperature reduction overlooks transient heat penetration, coating-side thermal loading and the exergy carried by heat across the crown. In this study, a three-dimensional transient finite element model of an aluminium–silicon diesel piston, with crown loading derived from Diesel-RK, was used to compare an uncoated piston with five ceramic top coats of 0.1–0.5 mm on a 0.1 mm nickel–chromium–aluminium bond coat. Against twenty measured temperatures of an uncoated piston, the model gave a mean absolute error of 3.32 K. At the common thickness of 0.3 mm, yttrium barium zirconate (YBZ) gave the strongest substrate shielding. Under a cold-initialised high-load step with cycle-mean gas-side conditions, it lowered the maximum substrate temperature by 48.87 K, reduced the cumulative convective crown heat transfer over 0–300 s by 25.52% and produced the longest top-coat-to-substrate thermal lag, 15.2 s. Cumulative crown exergy transfer decreased by 11.91% and gas-to-crown exergy destruction by 53.78%. When the crank-angle waveform was resolved, the gas-facing YBZ surface cycled by 149.3 K, whereas the buried NiCrAl/Al–Si interface varied by less than 0.1 K. Thicker YBZ coatings improved substrate protection but raised the top-coat temperature and the temperature difference across the ceramic; all five thicknesses were Pareto non-dominated, so the preferred thickness depends on allowable coating-side limits. The results provide a thermal screening basis for piston coatings, while mechanical integrity and durability require separate assessment.
No takes yet. Share an insight, caveat, or question.
Khan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: