The production of Portland cement accounts for approximately 8% of global anthropogenic carbon dioxide emissions. Incorporating biogenic carbon into concrete can reduce clinker use and valorise agricultural and forestry residues. In this study, hardwood (HW) and cocoa pod husk (CP) biochars treated at pyrolysis temperatures (PTs) of 300°C (T300) or 700°C (T700) were evaluated. The biochars were incorporated at rates of 0% to 3.0% by weight of cement across 25 mix designs and concrete specimens were tested at 7, 14 and 28 days. The use of 1.5% HW pyrolysed at 700°C led to the highest 28-day compressive strength (39.0 MPa), exceeding that of the control (35.0 MPa) by 11.4%. For this mix, water absorption decreased to 5.20% (5.70% for the control). After post-heating exposure (600°C, 2 h) this mix retained 80% of strength (70% for the control). The key contribution was the feedstock × PT interaction: at a dosage of 1.5%, the T700 − T300 strength difference was +0.2 MPa for HW but +5.2 MPa for CP. The empirical response model gave R2 = 0.68 and a leave-one-out root mean square error of 1.61 MPa. Analysis of variance identified PT (partial η2 = 0.38), quadratic dosage (0.21) and feedstock × dosage interaction (0.18) as dominant effects. Fourier transform infrared spectroscopy, X-ray diffraction (XRD), scanning electron microscopy and thermogravimetric analysis supported pore-refinement and aromatised-carbon mechanisms. However, isothermal calorimetry, mercury intrusion porosimetry and quantitative XRD investigations are needed to confirm the mechanisms.
No takes yet. Share an insight, caveat, or question.
Ajibade et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: