Conventional lithium recovery from α-spodumene, a major hard-rock lithium mineral, requires thermal phase conversion at ∼1100 °C followed by treatment with hot, concentrated sulfuric acid at ∼250 °C. We report a room-temperature mechanochemical route, MELLT (mechanochemical extraction of lithium at low temperature), that activates α-spodumene by solid–solid ion exchange during ball milling with readily available solid reagents (CaO or Na2CO3) and enables lithium extraction by water and/or dilute acid leaching. Using an automated high-throughput robotic platform to develop secondary leaching conditions, we found that CaO is more than twice as effective as Na2CO3. Under the optimized SPEX/steel screening condition using a 1:0.95 α-spodumene:CaO molar ratio, CaO delivers near-complete lithium extraction after 3 h of milling but requires 0.06 M H2SO4 under the investigated laboratory conditions, compared with 0.03 M H2SO4 for the best-performing Na2CO3 leaching condition. In contrast, Na2CO3 permits partial lithium extraction with water alone (20–35%), with subsequent dilute-acid leaching increasing the total extraction to 85%. Solid-state NMR spectroscopy provides evidence for the formation of an amorphous aluminosilicate with γ-like short-range order and supports progressive Li → Na and Li → Ca exchange during milling. Synchrotron X-ray scattering provides complementary information on milling-induced structural disorder. These results establish mechanochemical solid–solid ion exchange as a direct route for activating refractory aluminosilicate frameworks under ambient conditions.
No takes yet. Share an insight, caveat, or question.
Gvozdetskyi et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: