Answers are grounded in this paper and cite their sources.
A series of ZrC-SiC ceramic precursors (ZPSAP) with different Zr:Si molar ratios were prepared by solution blending, using zirconium bis(acetylacetonato) di-n-propoxide (Zr(acac)2(OPr)2) as the zirconium source, and a carbon-rich silicon-containing arylacetylene resin (PSA-HH) as the silicon and carbon source. The curing behavior, ceramization process, phase evolution, and oxidation resistance of the precursors and the ceramics were investigated by DSC, in situ FTIR, TGA, and XRD. The results show that after pyrolysis at 1600 °C, no crystalline ZrO2 was detected by XRD, indicating that carbothermal reduction in ZrO2 to ZrC had gone to completion. For all compositions, the final ceramics were dominated by crystalline ZrC, confirming that the carbon supplied by PSA-HH was sufficient to drive the reaction to completion. TGA testing showed that ZPSAP-0.5 exhibited virtually no change in mass in air at temperatures up to 1000 °C, indicating its excellent oxidation resistance. After isothermal oxidation in air at 1400 °C for 2 h, the mass changes were +1.47%, +5.47%, and +3.78% for Zr:Si = 2:1, 1:1, and 1:1.5, respectively, confirming that Zr:Si ≥ 1:1 sustains a compact m-ZrO2 scale, whereas excess SiC (1:2) causes scale cracking and breakaway oxidation.
No takes yet. Share an insight, caveat, or question.
Xu et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: