Ba 0.8 Sr 0.2 TiO 3 (BST) ceramics were prepared using solid-state method and sintered at 1100–1300°C for 3 h. The effect of sintering temperature on Structural, microstructure, dielectric, and electrical properties were investigated using X-ray diffraction (XRD), Rietveld refinement, Williamson-Hall analysis, FESEM, dielectric spectroscopy, and impedance measurements. XRD confirmed perovskite structure without detectable secondary crystalline phases. The principal diffraction peak FWHM decreased from 0.298 o to 0.104 o, while FESEM revealed grain growth from 0.43 to 4.15 µm. Dielectric measurement showed temperature dependent changes in dielectric constant and dielectric loss, with the dielectric maximum occurring at 80 o C. Modified Curie -Weiss analysis yielded a diffuseness exponent of 1.41 for BST1300, suggesting a diffuse dielectric transition. Impedance spectroscopy revealed non-ideal electrical relaxation, represented by a resistor-constant phase element equivalent circuit. Frequency dependent AC conductivity further demonstrated the influence of sintering induced microstructural evolution on electrical transport in BST ceramics.
No takes yet. Share an insight, caveat, or question.
Shankar et al. (2026) studied this question.
Synapse has enriched 8 closely related papers on similar clinical questions. Consider them for comparative context: