In this study, epoxy and epoxy‐kenaf fiber hybrid composites reinforced with nano‐titanium dioxide (TiO 2) and nano‐titanium diboride (TiB 2) were fabricated and systematically evaluated at filler loadings of 2–10 wt% to investigate their mechanical and thermal performance. The results showed that tensile strength, Young's modulus, and microhardness increased progressively with filler loading up to an optimum of 6 wt%, beyond which marginal reductions occurred due to particle agglomeration. At the optimum filler content for mechanical performance, epoxy‐kenaf‐TiO 2 composites achieved a tensile strength of 105 MPa, Young's modulus of 5.6 GPa, and microhardness of 38 HV. Superior mechanical performance was obtained for epoxy‐kenaf‐TiB 2 composites, which exhibited a maximum tensile strength of 130 MPa, Young's modulus of 7.0 GPa, and microhardness of 52 HV. Thermal conductivity showed only small changes with ceramic filler loading, whereas incorporating woven kenaf slightly reduced it relative to the corresponding ceramic‐filled epoxy composites.
No takes yet. Share an insight, caveat, or question.
Rajendra et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: