Over the last several years, researchers have noted some drawbacks to the basic Superpave test methods for assessing modified binders. This study compared atomic force microscopy (AFM), sessile drop (SD) surface free energy calculations, and the Texas Boiling Test (TBT) for characterizing binder surfaces and binder–aggregate moisture-related properties. Eighteen asphalt binders (PG 64-22, PG 70-22, and PG 76-22 from six sources) and eight aggregates (sandstone, limestone, dolomite, and novaculite, each from two quarries) were evaluated. The apparent DMT modulus from AFM ranged from 125 MPa (S5B1) to 765 MPa (S2B3). In the TBT, the S4B3–NV2 combination had the highest visually estimated coating retention (90%). The calculated dry work of adhesion ranged from 86.5 mJ/m2 (S2B2–NV1) to 174.5 mJ/m2 (S6B3–LS2). The water-induced debonding energy ranged from 7.9 mJ/m2 (S2B2–LS2) to 55.7 mJ/m2 (S5B1–NV2), where a lower value indicates a smaller driving force for stripping. The AFM images showed differences in bee-like surface morphology among binder sources. The methods ranked the materials differently, and no single binder performed best across all endpoints. Evaluating the three methods together shows which binder properties and binder–aggregate interactions each method can and cannot capture, which supports better-informed material selection and further study of moisture damage.
No takes yet. Share an insight, caveat, or question.
Sadat et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: