Corrosion significantly affects the durability and maintenance costs of metallic structures in saline environments. This study compared the corrosion behavior of ASTM A36 carbon steel, galvanized steel, aluminized steel, and 430F and 304L stainless steels under a six-week modified salt-spray exposure protocol incorporating daily heating (35 ± 2^∘ C, 5% NaCl saline solution) and cooling cycles. Specimens were positioned at 30^∘ and 45^∘, and corrosion was assessed through visual inspection and gravimetric measurements. Among the specimens tested, A36 exhibited the highest mass loss, whereas the coated steels showed intermediate values and the stainless steels the lowest. Differences between inclination angles were also observed, although the absence of independent replicates limits general conclusions. Expressing mass loss as a percentage of initial mass and per unit nominal surface area provided complementary measures of material degradation. The extended exposure period revealed changes in mass-loss trends after four weeks for the coated steels, highlighting the importance of monitoring corrosion over time.
No takes yet. Share an insight, caveat, or question.
Carvalho et al. (2026) studied this question.
Synapse has enriched 8 closely related papers on similar clinical questions. Consider them for comparative context: