Layered transition metal dichalcogenides can reversibly accommodate different alkali ions, yet their transport kinetics depend strongly on alkali identity and the associated structural evolution. CrSe2 can host one Li or Na ion per formula unit, but their relative kinetic accessibility during electrochemical intercalation and deintercalation and chemical deintercalation has not been established. Here, we use an optimized route to prepare O1−LiCrSe2 and O3−NaCrSe2 for a matched Li−Na kinetic comparison. Operando diffraction and composition-resolved chemical deintercalation distinguish an O1-retaining Li pathway from an O1/O3 structural transformation for Na. At 1 C, CrSe2||Li and CrSe2||Na delivers comparable capacities of 127 and 128 mAh g−1, respectively. At 25 C, CrSe2||Na retains 70% of its 1 C capacity, corresponding to 89 mAh g−1, whereas CrSe2||Li retains 55%, corresponding to 70 mAh g−1. Under the same chemical-deintercalation protocol, the iodine-consumption endpoint for the nominal alkali-free composition is reached after 8.1 h for NaCrSe2 and 26.9 h for LiCrSe2, respectively. The lower electrochemical polarization and calculated migration barrier for Na in NaCrSe2, 0.41 eV compared with 0.48 eV for Li in LiCrSe2, further support this kinetic ordering. These results establish greater kinetic accessibility for Na than Li within the layered CrSe2 framework despite the more extensive structural rearrangement associated with Na transport.
No takes yet. Share an insight, caveat, or question.
Li et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: