This study evaluated how the polymerization mechanism affects depth-dependent microhardness and shear bond strength to primary molar dentin. Three materials were tested: a conventional light-cured flowable composite, a light-cured bulk-fill composite and a self-cured bulk-fill composite. Each material was placed as a single increment, and Vickers microhardness was measured at 2.0, 3.0, and 4.0 mm (n = 10 per group). For shear bond strength testing, forty primary molars were assigned to four bonding groups (n = 10): the two light-cured composites were bonded with a universal adhesive, and the self-cured composite with either the universal adhesive combined with a dual cure activator or its dedicated primer. The interaction between material and depth was significant: microhardness decreased substantially with depth in the conventional composite, whereas the decrease was smaller in both bulk-fill materials and did not differ between them. Shear bond strength differed significantly among the groups (p < 0.0001), being highest in the self-cured composite with its dedicated primer (median 20.4 MPa) and lowest for the conventional composite (8.9 MPa), while the light-cured bulk-fill composite and the self-cured composite with the universal adhesive did not differ. Within the limitations of this study, the microhardness of the self-cured composite appeared less dependent on depth than that of the conventional composite and comparable with that of the lightcured bulk-fill composite, and its bond strength depended on the adhesive system used. This material may be of interest for restorations of primary molars in which light delivery is limited.
No takes yet. Share an insight, caveat, or question.
Kim et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: