Silicon anodes suffer from severe volume expansion and unstable solid electrolyte interphase (SEI), which limit their use in both liquid and solid‐state batteries. Here, a two‐dimensional siloxene‐based LP@SONS, is constructed by anchoring polypyrrole nanoparticles and lithiated‐Nafion onto siloxene nanosheets. This architecture combines electron‐conducting pathways with a Li + ‐selective ion‐sieving layer, homogenizing Li + flux, restricting anion/solvent penetration, and buffering strain. The stable and compositionally identical platform enables direct comparison of SEI evolution in liquid and solid electrolytes. In liquid cells, the SEI grows in a bulk‐permeated (3D) manner, whereas solid electrolytes confine growth to a planar solid–solid contact, yielding a LiF‐rich, planar‐confined (2D) SEI that passivates rapidly. Remarkably, LP@SONS promotes thinner, more uniform, LiF‐rich interphases in both systems. As a result, it delivers high reversible capacity, excellent rate capability, and long‐term cycling in liquid and solid‐state batteries, with only ∼5% thickness expansion after 100 cycles. This work clarifies how electrolyte contact geometry governs SEI dimensionality and offers an interfacial engineering strategy for high‐capacity anodes.
No takes yet. Share an insight, caveat, or question.
Hu et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: