SnO2 serves as a leading electron transport material in n–i–p perovskite solar cells (PSCs), yet its practical deployment is constrained by interfacial defects and energy-level mismatch. Herein, two naphthalene diimide (NDI) derivatives—DPNDI with pyridine terminals and NDI-N with dimethylamino terminals—are introduced at the SnO2/perovskite buried interface to investigate the effects of terminal groups on interfacial chemistry, crystallization, and charge dynamics. Theoretical calculations and X-ray photoelectron spectroscopy (XPS) confirm that DPNDI coordinates Pb2+ via pyridine N, while NDI-N coordinates via carbonyl O. Both form a dipole layer that retards crystallization, reduces defects, and minimizes voids and strain. NDI-N has a larger dipole due to intramolecular charge transfer from the dimethylamino groups to the NDI backbone, which improves SnO2 conductivity and reduces the conduction band offset to 0.08 eV, facilitating electron extraction. Consequently, the power conversion efficiency (PCE) increases from 19.88% (control) to 21.81% (DPNDI PSCs) and 24.17% (NDI-N PSCs). Unencapsulated NDI-N devices show superior storage stability, retaining 68.97% of initial PCE after 1000 h in N2 vs 50.22% for control. Under continuous maximum power point tracking (MPPT) in air, however, the encapsulated control device retains only 87.74% of its initial efficiency after 500 h, markedly lower than the 92.67% retained by encapsulated NDI-N devices.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: