Natural fibers are replacing synthetic fiber in composite applications because of their biodegradability, lightweight, low cost, and availability. However, the variability of mechanical properties due to the hydrophilic nature and poor adhesion with the hydrophobic matrix limits the widespread application. This study investigates the effects of chemical treatment of fiber on enset fiber-reinforced epoxy composite, fabricated using the hand lay-up method. Enset fiber was treated involving a constant concentration of sodium hypochlorite (NaOCl) as a bleaching pretreatment, followed by various concentration of NaOH and benzoyl chloride. A Taguchi L9 orthogonal array with four factors (NaOH concentration (A), benzoyl chloride concentration (B), drying temperature (C), and immersion time (D)) and three levels was designed to optimize the parameters based on mechanical, structural, and thermal properties. XRD, SEM, FTIR, TGA, and DTG were used for characterization. L2 achieved a crystallinity index of 65.79% and 8.11% residual mass at 600°C, while L1 showed optimum tensile strength (37 MPa) and flexural strength (57 MPa). The Taguchi signal-to-noise ratio analysis identified A1B2C3D1 for tensile and A2B2C1D1 for flexural strength as the optimum factor-level combination for mechanical performance. The analysis indicated that treatment conditions must be carefully controlled to achieve a balance between mechanical performance and fiber modification.
No takes yet. Share an insight, caveat, or question.
Teriya et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: