Continuous flax fiber-reinforced polylactic acid (PLA) composites were produced by fused filament fabrication (FFF) using a customized in-nozzle impregnation head. The effects of hatch spacing (1.0–2.0 mm) and layer thickness (0.4–0.8 mm) were investigated through a 3 × 3 full factorial design. The constituent materials and printed composites were characterized by thermogravimetric analysis (TGA), differential scanning calorimetry (DSC), X-ray diffraction (XRD), and Fourier transform infrared spectroscopy (FT-IR). Tensile strength ranged from 47.35 to 68.48 MPa and flexural strength from 66.52 to 89.79 MPa across the nine processing conditions, compared with 55 and 56 MPa for the neat PLA filament. The highest strengths were obtained at a hatch spacing of 1.0 mm and a layer thickness of 0.4 mm, with a calculated fiber volume fraction of 69%. Analysis of variance (ANOVA) showed that hatch spacing accounted for more than 60% of the variation in both properties, compared with 26–30% for layer thickness. Scanning electron microscopy (SEM) of the fracture surfaces revealed fiber pull-out and interfacial debonding. PLA penetration was confined mainly to the outer region of the flax yarn, leaving the inner fibers insufficiently impregnated, which likely restricted load transfer, particularly under tensile loading. Reducing hatch spacing improved the mechanical response more strongly than reducing layer thickness, indicating that the overlap of deposited tracks is a key consideration in in-nozzle impregnation of continuous flax/PLA composites.
No takes yet. Share an insight, caveat, or question.
Atagür et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: