Carbon fibre-reinforced aluminium laminates (CARALLs) combine the high specific stiffness of carbon-fibre composites with the ductility and damage tolerance of aluminium alloys, although their mechanical performance is strongly influenced by the integrity of the metal-composite interfaces and by the manufacturing route adopted for specimen preparation. In this work, CARALL laminates consisting of AA2017 aluminium sheets, CYCOM® 950-1 carbon/epoxy prepreg and 3M™ Scotch-Weld™ AF 163-2 structural adhesive films were manufactured by hand lay-up, vacuum bagging and oven curing. Specimens were subsequently extracted by abrasive waterjet (AWJ) cutting. Preliminary cutting trials were performed at water pressures of 100, 200 and 300 MPa while keeping the remaining process parameters constant. At the lower pressure levels, extensive delamination and interfacial separation were observed. At 200 MPa, some specimens appeared macroscopically intact, although SEM observations revealed local debonding at the aluminium-adhesive interface and delamination within the CFRP sublaminate. A pressure of 300 MPa was therefore adopted for the specimens subsequently subjected to fatigue testing. The results highlight the sensitivity of CARALL laminates to AWJ-induced damage and underline the importance of controlling specimen edge integrity when assessing their fatigue response.
No takes yet. Share an insight, caveat, or question.
Parodo et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: