Polytetrafluoroethylene (PTFE) is renowned for its chemical inertness and thermal stability, making it suitable for synthesizing products exposed to harsh conditions. However, its inertness hinders adhesion to other materials or the deposition of coatings. This requires an increase in surface energy. A suitable method is sequential treatment with hydrogen plasma and oxygen plasma afterglow. Systematic experiments were performed to determine the optimal parameters. PTFE was exposed to hydrogen plasma sustained by an inductively coupled radiofrequency (RF) discharge in the H mode. The gas pressure was 21 Pa and the RF power was 500 W. The hydrogen-plasma-pretreated samples were then exposed to O2 plasma flowing afterglow at a neutral oxygen atom density of 4.4 × 1021 m–3. The treatment times ranged from 10 ms to 3 s for hydrogen plasma and from 10 ms to 30 s for oxygen afterglow. The water contact angle (WCA) reached values below 10°. The loss of hydrophilicity at longer treatment times was attributed to thermal effects and etching. The optimal conditions were at a hydrogen-ion fluence of 6 × 1019 m–2 and an oxygen-atom fluence of 7 × 1022 m–2. Hydrophobic recovery was marginal, with WCA increasing by only about 15° after four days of storage.
No takes yet. Share an insight, caveat, or question.
Zaplotnik et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: