We present the decoration of a mesoporous carbon matrix with a LiCl/KCl eutectic by hand milling or incipient wetness impregnation. Nitrogen isotherms indicated that the latter favoured the salt impregnation of the pores. Electron microscopy revealed cubic nanoparticles ranging from 100 to 1000 nm covering the matrix. Powder X-ray diffractometry confirmed the presence of LiCl and KCl crystals. The characteristic melting peak of the LiCl/KCl eutectic was detected at 354 ºC by differential scanning calorimetry. The LiCl/KCl decorated matrices were then melt-impregnated with LiBH 4. Nitrogen isotherms indicated limited LiCl/KCl impact on LiBH 4 pore filling, beneficial for wet-impregnated matrices but detrimental to ground matrices. SEM observations revealed partially melted nanocrystals at the matrix surface. Calorimetry of the decorated materials exhibited a broader and less intense LiBH 4 decomposition peak shifted toward higher temperatures (348 ºC), while no melting peak was observed and the transition peak shifted sharply toward lower temperatures (70 ºC). Powder X-ray diffractometry evidenced the disappearance of KCl and suggested the formation of LiK(BH 4) 2 after impregnation with LiBH 4. Volumetric studies revealed that the onset of hydrogen release was shifted toward lower temperatures for wet-impregnated samples, but higher temperatures were required to finish the decomposition of ground samples. No effect on the system´s reversibility was observed. XRD and DSC could not demonstrate the presence of the LiH/LiCl/KCl eutectic after cycling. However, SEM observation revealed the formation of needle-shaped crystals after decomposition.
No takes yet. Share an insight, caveat, or question.
Garanzini et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: