Answers are grounded in this paper and cite their sources.
ZnS 1-x Te x thin films were deposited on glass substrates by thermal co-evaporation under high-vacuum conditions. The effect of substrate temperature on composition, crystal structure, optical properties, photoluminescence, and spectral photoconductive response was investigated. Energy-dispersive X-ray spectroscopy showed that the Te fraction varied markedly with substrate temperature, with x values of 0.90, 0.67, 0.13, and 0.39 for films deposited at 100, 150, 200, and 250 ºC, respectively. X-ray diffraction revealed that the films were polycrystalline, with a cubic zinc-blende structure and preferred (111) orientation. Optical characterization showed band-gap energies ranging from2.19 to 3.13 eV across the investigated sample series. The photoluminescence spectrum of the film deposited at 100ºC exhibited a broad emission band that was fitted with two Gaussian components centered at approximately 515 and 579 nm. Photoconductivity measurements revealed broad spectral responses that depended on substrate temperature: films deposited at 100 and 150ºC exhibited a photoconductive response over almost the entire visible range, whereas the film deposited at 250ºC showed a response shifted toward longer wavelengths. These results demonstrate that substrate temperature provides an effective means of modifying the composition and optoelectronic response of ZnS(1-x)Tex thin films and support further investigation of these films as potential materials for broadband visible photodetection.
No takes yet. Share an insight, caveat, or question.
Andrade et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: