Answers are grounded in this paper and cite their sources.
Deicing salts are known to cause surface scaling in concrete construction in freeze-thaw (F-T) conditions. To evaluate the chloride resistance of concrete incorporating General Use Limestone (GUL) cement with Ground Granulated Blast-Furnace Slag (GGBFS) under realistic field conditions, the specimens were exposed to drying conditions after 4 days of standard curing, they were also exposed to more aggressive conditions involving chloride penetration and F-T salt scaling conditions. Surface samples of concrete before and after F-T salt scaling were further analyzed using thermogravimetric analysis (TGA) and X-ray diffraction (XRD) to assess phase evolution. Results show that compressive strength increases by 24.3% with GGBFS content up to 30%, then decreases at 40-50% but remains within 40-50 MPa. Increasing GGBFS content significantly reduces chloride penetrability based on the RCPT and resistivity tests. After specimens are subjected to 50% RH drying environment, which induces surface carbonation and converts portlandite and ettringite into stable carbonate phases. In F-T cycling with deicing salts, deterioration is governed by the carbonated surface layer. When exposed to 3% NaCl F-T cycles at 28 days, mixtures containing 10% GGBFS show the best resistance to surface scaling. By 40 days, the optimum GGBFS content is observed at 25%. Compared with 3% NaCl exposure, 3% CaCl 2 and 3% (NaCl:MgCl 2 ) (43:57) deicing salt solution reduces F-T salt scaling. These findings highlight that curing history and deicer solutions influence the performance of GUL-GGBFS concrete and enable the durability benefits of GGBFS to be achieved in cold region infrastructure.
No takes yet. Share an insight, caveat, or question.
Ma et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: