High-density polyethylene (HDPE) is entering small-craft construction, but its thermal expansion is ten times that of steel and its stiffness falls steeply above 60 °C, so sunlight can deform welded panels permanently. Two campaigns following the MIL-STD-810H 505.7 Procedure I A1 cycle (1120 W/m2) tested 500 × 500 × 10 mm welded HDPE plates, T-stiffened plates and open-sided boxes. Surface temperatures reached 78–115 °C against 49 °C chamber air. Deflections measured both at peak irradiance and after cooling separate two components: a reversible thermal bow of 5–6 mm and a permanent set of 6–9 mm, concave towards the lamps (19 mm on the hottest plate), about 70% of which appeared in the first cycle. A thermo-viscoelastic plate model with the actual support condition reproduces the surface temperatures within 3 K and the reversible bow, but accounts for less than 30% of the permanent set, as does a Norton-creep model in ANSYS. The set is described instead by a measured inherent curvature of 0.19–0.29 m−1, attributed to irreversible shrinkage of the heated face and release of welding residual stress, which gives the order of the box deflection (5.3–7.9 mm against 5–8 mm measured) and doubles at 111–115 °C. Sizing guidance by temperature, combining this curvature, sustained-load creep and a model factor of 2.0, is given.
No takes yet. Share an insight, caveat, or question.
Kang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: