Bond-test results depend on the complete test configuration and the component that fails. This study reanalyzes 296 specimen-level results for five commercial and three laboratory-proportioned repair mortars tested in direct tension, flexural tension, direct shear, and slant shear. Comparisons emphasize the common ages of 7 and 28 days; initial results are descriptive because direct tension was tested at 2 days and the other methods at 1 day. One mortar batch was used per mortar–configuration–age condition, and one concrete batch per configuration. Consequently, statistical decompositions and resampling describe the tested batches rather than independently replicated treatment effects. On the log-strength scale, the descriptive partial interaction measure was 0.883 at 7 days and 0.494 at 28 days; after removing direct shear, it was 0.906 and 0.464, respectively. AI-2 had the largest observed cell means, without demonstrated superiority in every comparison. At 28 days, direct-shear failures occurred in the substrate for seven mortars, so those values represent substrate-limited system capacity rather than measured interfacial strength. Direct tension remained interfacial among the specimens successfully tested. Differences in preparation, geometry, loading rate expressed as stress, and substrate batch prevent attribution to stress state alone. The results support configuration-specific interpretation and systematic reporting of failure location, while microscopy provides only localized qualitative observations.
No takes yet. Share an insight, caveat, or question.
Kudlanvec et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: