This study demonstrates enhanced fracture toughness in a glass ceramic infused with muscovite, suggesting improvements for dental prostheses.
The principal objective of this studywas to produce and characterize a machinable glass ceramic containing muscovite-mica as the main crystalline phase to be used as a dental restorative material. The secondary objective was to evaluate the use of muscovite-mica to improve machinability and generate a toughening mechanism in the experimental glass ceramic. After fine milling of a feldspathic glass frit was milled and then mixed with muscovite-mica, die-pressed, and sintered under vacuum at 850 to 1,150 °C. The resulting sintered composite was characterized by X-ray diffraction, scanning electron microscopy, and had its fracture toughness evaluated by micro-indentation. The results were as follows: (a) improved thermal stability of muscovite-mica crystals in the composite; (b) improved leucite crystallization in the feldspathic glass matrix by increasing sintering temperature in the studied range ; (c) the composites consisting of glass + 10% muscovite and glass + 20% muscovite sintered at 1,050°C presented fracture toughness values of 9.0 ± 1.2 and 8.4 ± 0.6 MPa.m1/2, respectively, which are higher than those found in the literature for glass ceramics. Feldspar frit blocks with addition of muscovite-mica (up to 20%) can be densified at temperatures between 1,050 and 1,150°C. This material was stable at a temperature substantially higher than the stability limit of pure muscovite and also showed indentation fracture toughness values greater than those reported in the literature for other glass ceramics.
No takes yet. Share an insight, caveat, or question.
PIETOSO et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: