Answers are grounded in this paper and cite their sources.
This paper studies the influence of FDM 3D printing process parameters on the size error of printed parts based on an orthogonal experiment. The main objective is to investigate the influence of four factors, including printing layer height, printing speed, substrate temperature, and nozzle temperature, at different levels on the size error of printed parts. The experimental results are analyzed using the method of range analysis, and the main order of influence of each factor on size error is determined. The results show that the main order of influence of each factor on size error is: printing layer height > printing speed > nozzle temperature > substrate temperature. The optimal process parameter combination is determined as a printing layer height of 0.1 mm, printing speed of 40 mm/s, substrate temperature of 65 °C, and nozzle temperature of 190 °C. Furthermore, as the printing layer height increases, the size error gradually increases, while as the substrate temperature increases, the size error tends to decrease. Finally, the experimental comparison verifies that the optimized process parameter combination can effectively reduce the size error of printed parts, and the size deviation reduction rate is 13.8%, providing a reference for the optimization of FDM 3D printing process parameters.
No takes yet. Share an insight, caveat, or question.
Mi et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: