Air-dried density, weight loss (WL), impact bending strength (IBS), Shore-D hardness, and thermal conductivity values were determined for heat-treated poplar (Populus nigra L.) and beech (Fagus orientalis Lipsky) wood and compared with those for untreated samples. The test samples were heat-treated at 140, 160, 180, and 200 °C for 2 h. The results showed that density decreased and WL increased with increasing temperature for all temperatures. Additionally, during the heat treatment, the IBS increased in beech wood samples at 140 °C, but at higher temperatures, these values gradually decreased in both wood species. The highest decline in IBS values, found at a temperature of 200 °C, was 66.5% for beech and 55.7% for poplar. The Shore-D hardness of both wood species increased after heat treatment and regarding beech wood, the hardness increasing rate at temperature at 140 °C, 160 °C, 180 °C and 200 °C, 8.94%, 14.19%, 8.27% and 11.7%, respectively according to control samples. Regarding poplar wood, hardness increasing rates were 6.20% at 140 °C, 4.41% at 160°C, 5.88% at 180°C and 5.31% at 200°C according to control samples. The thermal conductivity of poplar and beech wood samples decreased after heat treatment, except for samples heat treated at 160 °C.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Perçin et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: